Background: Big injection molder from Europe, never used purging agent in the past. Needed a solution for Polyamide color change (black to white) in order to reduce machine downtime and reducing scrap rate.

The process & results can be clearly seen below:

 Purge material PolyamideRamclean 204
Cylinder capacity0.5 Kg0.5 Kg
Waste per cleaning cycle/ monthly waste10-13 Kg0.5 Kg